| Product Features | Wear Resistance, Corrosion Resistance, Belongs To The Special Alloy, Hardness In HRC≥57, Alloy Parent Full Melt, Improve The Density, Hardness. |
|---|---|
| Temperature Resistance | Temperature Limit 600℃ |
| Alloy Layer Thickness | ≧1.8mm |
| Alloy Layer Hardness | HRC≥57 |
| Advantage | Elliptic Flat Angle Process |
| Product Features | Wear Resistance, Corrosion Resistance, Belongs To The Special Alloy, Hardness In HRC≥57, Alloy Parent Full Melt, Improve The Density, Hardness. |
|---|---|
| Temperature Resistance | Temperature Limit 600℃ |
| After Warranty Service | 12 Months After Shipment |
| Advantage | Long Service Life |
| Hs Code | 8477900000 |
| Product Features | Wear Resistance, Corrosion Resistance, Belongs To The Special Alloy, Hardness In HRC≥57, Alloy Parent Full Melt, Improve The Density, Hardness. |
|---|---|
| Temperature Resistance | Temperature Limit 600℃ |
| After Warranty Service | 12 Months After Shipment |
| Advantage | Long Service Life |
| Hs Code | 8477900000 |
| Product Features | Wear Resistance, Corrosion Resistance, Belongs To The Special Alloy, Hardness In HRC≥57, Alloy Parent Full Melt, Improve The Density, Hardness. |
|---|---|
| Temperature Resistance | Temperature Limit 600℃ |
| Alloy Layer Hardness | HRC≥57 |
| Hs Code | 8477900000 |
| Liner Type | Nickel Chrome Tungsten Composite Liner |
| Product Features | Wear Resistance, Corrosion Resistance, Belongs To The Special Alloy, Hardness In HRC≥57, Alloy Parent Full Melt, Improve The Density, Hardness. |
|---|---|
| Temperature Resistance | Temperature Limit 600℃ |
| Alloy Layer Thickness | ≧1.8mm |
| Alloy Layer Hardness | HRC≥57 |
| Advantage | Elliptic Flat Angle Process |
| Main Material | NiCrW Alloy (Ni60 Based On The Addition Of CrC And CrB |
|---|---|
| Product Features | Wear Resistance, Corrosion Resistance, Belongs To The Special Alloy, Hardness In HRC≥57, Alloy Parent Full Melt, Improve The Density, Hardness. |
| Temperature Resistance | Temperature Limit 600℃ |
| Alloy Layer Thickness | ≧1.8mm |
| Alloy Layer Hardness | HRC≥57 |
| Material | 38CrMoAlA,42CrMo,9Cr18MoV |
|---|---|
| Application Field | Household,Agriculture,Industry,Building,Auto Parts |
| Applied Polymers | PE,PA,PET,PVC,PC,ABS,PBT,PEEK,Teflon |
| Screw Treatment | Nitrided,Bimetallic,PTA,HOVF,Tool Steel,HSS,PM Steel |
| Model Number | 90MJ II, 120MJ II, 150MJ II, 180MJ II, 210MJ II, 270MJ II, 320MJ II, 390MJ, 500MJ, 610MJ, 720MJ, 950MJ, 1200MJ |
| Material | 38CrMoAlA,42CrMo,9Cr18MoV |
|---|---|
| Application Field | Household,Agriculture,Industry,Building,Auto Parts |
| Applied Polymers | PE,PA,PET,PVC,PC,ABS,PBT,PEEK,Teflon |
| Screw Treatment | Nitrided,Bimetallic,PTA,HOVF,Tool Steel,HSS,PM Steel |
| Reinforced Additives | Less Than 65% Glass Fibre |
| Type | Twin Bimetallic Conical Screw And Barrel |
|---|---|
| Base Material | 38CrMoAlA,SACM645,42CrMo,SKD61,GH113,etc |
| Bimetallic Screw Process | Spray Welding |
| Bimetallic | Fe-based,Ni-based,Tungsten Carbide |
| End Products | Recycled PE,PP,ABS,EPS,XPS,PC Pelletizing Extruder |
| Material | Bimetallic Alloy |
|---|---|
| Screw Diameter | 20-220mm |
| Mould Clamping Force | 250-3200T |
| Nitrided Layer Depth | 0.5-0.8mm |
| Hard Chorme Plating | >=950 |