Material | 38CrMoAlA,42CrMo,9Cr18MoV |
---|---|
Application Field | Household,Agriculture,Industry,Building,Auto Parts |
Applied Polymers | PE,PA,PET,PVC,PC,ABS,PBT,PEEK,Teflon |
Screw Treatment | Nitrided,Bimetallic,PTA,HOVF,Tool Steel,HSS,PM Steel |
Reinforced Additives | Less Than 65% Glass Fibre |
Name | Screw Barrel |
---|---|
Product Features | Wear Resistance, Corrosion Resistance, Belongs To The Special Alloy, Hardness In HRC≥57, Alloy Parent Full Melt, Improve The Density, Hardness. |
Temperature Resistance | Temperature Limit 600℃ |
Alloy Layer Thickness | ≧1.8mm |
Alloy Layer Hardness | HRC≥57 |
Assembly Structure | Separate Type Extruder |
---|---|
Engagement System | Full Intermeshing |
Screw Channel Structure | Deep Screw |
Diameter | 12-350mm |
Screw Design | Parallel Twin Screw |
Name | Screw Barrel |
---|---|
Product Features | Wear Resistance, Corrosion Resistance, Belongs To The Special Alloy, Hardness In HRC≥57, Alloy Parent Full Melt, Improve The Density, Hardness. |
Temperature Resistance | Temperature Limit 600℃ |
Alloy Layer Thickness | ≧1.8mm |
Alloy Layer Hardness | HRC≥57 |
Main Material | NiCrW Alloy (Ni60 Based On The Addition Of CrC And CrB |
---|---|
Product Features | Wear Resistance, Corrosion Resistance, Belongs To The Special Alloy, Hardness In HRC≥57, Alloy Parent Full Melt, Improve The Density, Hardness. |
Temperature Resistance | Temperature Limit 600℃ |
Alloy Layer Thickness | ≧1.8mm |
Alloy Layer Hardness | HRC≥57 |
Main Material | NiCrW Alloy (Ni60 Based On The Addition Of CrC And CrB |
---|---|
Product Features | Wear Resistance, Corrosion Resistance, Belongs To The Special Alloy, Hardness In HRC≥57, Alloy Parent Full Melt, Improve The Density, Hardness. |
Temperature Resistance | Temperature Limit 600℃ |
Alloy Layer Thickness | ≧1.8mm |
Alloy Layer Hardness | HRC≥57 |
Main Material | NiCrW Alloy (Ni60 Based On The Addition Of CrC And CrB |
---|---|
Product Features | Wear Resistance, Corrosion Resistance, Belongs To The Special Alloy, Hardness In HRC≥57, Alloy Parent Full Melt, Improve The Density, Hardness. |
Temperature Resistance | Temperature Limit 600℃ |
Alloy Layer Thickness | ≧1.8mm |
Alloy Layer Hardness | HRC≥57 |
Product Description | Screw Elements |
---|---|
Materials | W6542,Wr5,CPM10V,CPM9V And So On |
Hardness | Based On Different Materials |
Application | Parallel Twin Extruder |
Charactors | High Wear-Resistance,High Corrossion Resistance |
Product Description | Screw Elements |
---|---|
Materials | W6542,Wr5,CPM10V,CPM9V And So On |
Hardness | Based On Different Materials |
Application | Parallel Twin Extruder |
Charactors | High Wear-Resistance,High Corrossion Resistance |
Place Of Origin | Jiangsu,China |
---|---|
Material | 316L/X260/W6Mo5Cr4V2 Or Customized |
Spare Parts Type | Spare Parts For Twin Screw Exruder |
Application | Machinery Repair Shops,Food An Beverage Factory |
Center Distance | 26mm |