Features
Specifications
Standard: AISI, ASTM, BS, DIN, GB, JIS, Other,JIS,AISI,ASTM,GB,DIN,EN
Grade: Inconel 718
Thickness: 8mm-100mm
Place Of Origin: Jiangsu, China (Mainland)
Type: Tube / Pipe
Dimensions: 10-900MM
Length: 2m,3m Or As Required
Special Use: Cold Heading Steel
Delivery: 25-30 Days Subject To The Clients' Requirements And Quantity
Price Term: Ex-Work,FOB,CNF,CFR,CIF,FCA,DDP,DDU
Surface Treatment: Bright&smooth
Application: Structural Steel Bar
Highlight:

inconel 625 material

,

inconel 718 material

Basic Infomation
Place of Origin: Jiangsu, China (Mainland)
Brand Name: BLM-DX-1
Payment & Shipping Terms
Packaging Details: packed and labeled according to the regulations and customer's requests.Great care is taken to avoid any damage which might otherwise be caused during storage or transportation.
Delivery Time: 25-30 days subject to the clients' requirement and quantity
Payment Terms: Western Union, L/C, T/T
Supply Ability: 300 Ton/Tons per Month
Product Description

Inconel 718

Inconel 718 Chemical composition

 

Alloy % Ni Cr Fe Mo Nb Co C Mn Si S Cu Al Ti
718 Min. 50 17 balance 2.8 4.75             0.2 0.7
Max. 55 21 3.3 5.5 1 0.08 0.35 0.35 0.01 0.3 0.8 1.15

 

 

Inconel 718 Physical properties

 

Density 8.2 g/cm³
Melting point 1260-1340 ℃

 

 

Inconel 718 Alloy minimum mechanical properties in the roomtemperature

 

Alloy Tensile strength Rm N/mm² Yield strength R P0. 2N/mm² Elongation A 5 %

Brinell hardness

HB

Solution treatment 965 550 30 ≤363

 

 

718 Characteristic as below:

1.workability

2.High tensile strength,endurance strength,creep strength and rupture strength at 700℃.

3.High inoxidability at1000℃. 4.Steady mechanical performance in the low temperature.

5.Good welding performance.

 

 

Inconel 718 Metallurgical structure

 

718alloy is Austenitic structure, precipitation hardening generate "γ" made it excellent mechanical performance. G rain boundary generate "δ" made it the best plasticity in the heat treatment.

 

 

 

Inconel 718 Corrosion resistance

 

718 alloy with extremely resistance to stress corrosion cracking and pitting ability in high temperature or low temperature environments, especially the inoxidability in the high temperature.

 

 

Inconel 718 Application field:

1 . The elevated temperature strength, excellent corrosion resistance and workability at 700℃ properties

2 . made it use in a wide range of high requirement environments :Steam turbine ; Liquid-fuel rocket ; Cryogenic engineering

3.Acid environment

4.Nuclear engineering

 

 

965 Tensile Strength Inconel Nickel Alloy Inconel 718 Tube With Stress Corrosion Cracking Resistance 0

 

 

 

 

Recommended Products
Get in touch with us
Contact Person : Kara Liu
Tel : 0086-13914912658
Fax : 86-512-89598069
Characters Remaining(20/3000)